Deflection Temperature at 1.8 MPa (264 psi) 363 °C
685 °F
ASTM D648
Parker Chomerics PREMIER™ PEI-140 High Temperature Conductive Plastic for EMI Shielding
PEI-140 can provide up to a 65% cost reduction by eliminating secondary operations such as assembly, machining, painting/plating and the logistics that accompany these processes. The shielding effec..