Polymer Property : Deflection Temperature at 1.8 MPa (264 psi) = 348.3 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 175.7 °C
348.3 °F
ASTM D648
CRP Technology Windform® LX 2.0 Polyamide Composite
Processed by selective laser sintering (SLS). Windform® LX 2.0 has improved the already excellent performances of Windform® LX and this can be noticed from technical properties and sinterability ..