Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Deflection Temperature at 1.8 MPa (264 psi) = 344.1 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 173.4 °C
344.1 °F
ISO 75-2 TYPE A
CRP Technology Windform® XT 2.0 Polyamide-Carbon Fiber Composite
Processed by selective laser sintering (SLS). Windform® XT 2.0 is the evolution of the ground breaking high performance Windform® XT, the carbon fiber reinforced composite material, known for its..
Copyright © lookpolymers.com All Rights Reserved