Polymer Property : Deflection Temperature at 1.8 MPa (264 psi) = 321 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 321 °C
610 °F
ASTM D648
Performance Polymers IPS II PPL-C4150 PEKK (Polyetherketoneketone) Linear 30 % Glass Fiber Reinforced Molding Grade
Amber pelletsInformation provided by Infinite Polymer System II.
Deflection Temperature at 1.8 MPa (264 psi) 321 °C
610 °F
ASTM D648
Performance Polymers IPS II PPL-C4250 PEKK (Polyetherketoneketone) Linear 30% Carbon Fiber Reinforced Molding Grade
Black pelletsInformation provided by Infinite Polymer System II.