Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 32.0 - 34.0 °C | 89.6 - 93.2 °F | ASTM D648-07 |
Proto3000 Objet DurusWhite FullCure430 Polypropylene-like Prototyping Polymer Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 32.0 °C @Thickness 3.20 mm |
89.6 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP LUBRICOMP LCL33EXQ PEEK LNP* LUBRICOMP* LCL33EXQ is a compound based on Polyetheretherketone containing 15% Carbon Fiber, 15% PTFE. Added features of this material include: Wear Resistant, Easy Molding. |