Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 132.22 °C | 270.00 °F | ASTM D648 |
Lucent Polymers PC-1403 Polycarbonate, Extrusion/Blow Molding Grade Medium FlowAdd "R" for Added ReleaseAdd "U" for UVÂ StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 132.22 °C | 270.00 °F | ASTM D648 |
Lucent Polymers PC-1403FD Polycarbonate, FDA Compliant, Extrusion/Blow Molding Grade Medium FlowAdd "R" for Added ReleaseAdd "U" for UVÂ StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 132.22 °C | 270.00 °F | ASTM D648 |
Lucent Polymers PC-1406 Polycarbonate, Extrusion/Blow Molding Grade Medium FlowAdd "R" for Added ReleaseAdd "U" for UVÂ StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 132.22 °C | 270.00 °F | ASTM D648 |
Lucent Polymers PC-1406FD Polycarbonate, FDA Compliant, Extrusion/Blow Molding Grade Medium FlowAdd "R" for Added ReleaseAdd "U" for UVÂ StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 132.22 °C | 270.00 °F | ASTM D648 |
Lucent Polymers PC-1410 Polycarbonate, Injection/Extrusion Grade Medium FlowAdd "R" for Added ReleaseAdd "U" for UVÂ StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 132.22 °C | 270.00 °F | ASTM D648 |
Lucent Polymers PC-1410FD Polycarbonate, FDA Compliant, Injection/Extrusion Grade Medium FlowAdd "R" for Added ReleaseAdd "U" for UVÂ StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 132.22 °C | 270.00 °F | ASTM D648 |
Lucent Polymers PC-1418 Polycarbonate, Injection Grade High FlowAdd "R" for Added ReleaseAdd "U" for UVÂ StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 132.22 °C | 270.00 °F | ASTM D648 |
Lucent Polymers PC-1418FD Polycarbonate, FDA Compliant, Injection Grade High FlowAdd "R" for Added ReleaseAdd "U" for UVÂ StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 132.22 °C | 270.00 °F | ASTM D648 |
Lucent Polymers PC-1425 Polycarbonate, Injection Grade High FlowAdd "R" for Added ReleaseAdd "U" for UVÂ StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 132.22 °C | 270.00 °F | ASTM D648 |
Lucent Polymers PC-1428 Polycarbonate, Injection Grade High FlowAdd "R" for Added ReleaseAdd "U" for UVÂ StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 132.22 °C | 270.00 °F | ASTM D648 |
Lucent Polymers PC-1428FD Polycarbonate, FDA Compliant, Injection Grade High FlowAdd "R" for Added ReleaseAdd "U" for UVÂ StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 132.22 °C | 270.00 °F | ASTM D648 |
Lucent Polymers PC-FR0 Polycarbonate, Flame Resistant UV Stable/Weatherable, f1 RatedMelt Flow Adjustable for Application UL File Number: E213588Information provided by Lucent Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 132.22 °C | 270.00 °F | ASTM D648 |
Lucent Polymers PC-FR2 Polycarbonate, Flame Resistant Melt Flow Adjustable for ApplicationUL File Number: E213588Add "R" for Added ReleaseAdd "U" for UV StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 132.22 °C | 270.00 °F | ASTM D648 |
Lucent Polymers POM-100 Acetal Copolymer, General Purpose, Injection Grade Add "U" for UV StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 132.22 °C | 270.00 °F | ASTM D648 |
Lucent Polymers POM-270 Acetal Copolymer, Easy Flow, Injection Grade Add "U" for UV StabilizedInformation provided by Lucent Polymers, Inc. |