Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 115.56 °C | 240.01 °F | ASTM D648 |
Lucent Polymers PC/ABS-1003 Polycarbonate+ABS, Extrusion / General Purpose, Injection Grade Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc. |