Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 180 - 233 °C
356 - 451 °F
Average value: 205 °C Grade Count:35
Overview of materials for Polyethylene Terephthalate (PET), 20% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 20% Glass Reinforced". Specific grades with glass content between 15% ..