Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 185.6 °C | 366.1 °F | ASTM D648 Type B |
CRP Technology Windform® SP Polyamide-Carbon Fiber Composite for 3D Printing Processed by selective laser sintering (SLS). Windform® SP is a deep black composite polyamide that is a “Top” level material within the polyamide Windform® materials for additive manufacturing.. |