Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 82.22 °C | 180.0 °F | ASTM D648 |
Lucent Polymers ABS-45T Acrylonitrile Butadiene Styrene, High Impact Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 82.22 °C | 180.0 °F | ASTM D648 |
Lucent Polymers PC/PBT-0820 Polycarbonate+PBT, Injection Grade Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 82.22 °C | 180.0 °F | ASTM D648 |
Lucent Polymers PC/PBT-1020 Polycarbonate+PBT, General Purpose, Injection Grade Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 82.22 °C | 180.0 °F | ASTM D648 |
Lucent Polymers TPP-140 Polypropylene, Homopolymer, 40% Talc Filled Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |