Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 76.67 °C | 170.0 °F | ASTM D648 |
Lucent Polymers TPP-120 Polypropylene, Homopolymer, 20% Talc Filled Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 76.67 °C | 170.0 °F | ASTM D648 |
Lucent Polymers TPP-230 Polypropylene, 30% Talc Filled, Impact Modified Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 76.67 °C | 170.0 °F | ASTM D648 |
Lucent Polymers TPP-340 Polypropylene, 40% Talc Filled, Impact Modified Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |