Polymer Property : Deflection Temperature at 1.8 MPa (264 psi) = 168.8 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 76.00 °C
168.8 °F
ASTM D-648
Axiall HH-2000 Rigid PVC, Molding
Georgia Gulf HH-2000 is a high heat/high flow injection molding grade PVC alloy with a price/performance niche between high flow vinyl and utility engineering thermoplastics. It combines excellent ..