Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 68.33 °C | 155.0 °F | ASTM D648 |
Lucent Polymers CPP-130 Polypropylene Homopolymer, 30% Calcium Carbonate Filled Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 68.33 °C | 155.0 °F | ASTM D648 |
Lucent Polymers CPP-140 Polypropylene Homopolymer, 40% Calcium Carbonate Filled Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |