Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 64.4 °C | 148 °F | ASTM D648 |
RheTech Products HP534-00 22% Talc Reinforced High Performance Polypropylene Copolymer, Natural Applications: Door trim panelsCenter consolesSteering columnsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 64.4 °C | 148 °F | unannealed; ASTM D648 |
KYDEX® 321 Co-Extruded High Impact Fire Rated Sheet Features:Metallic cap, black, gray or off-white substrateThickness ranging from 3.18 mm to 8.9 mmTextures: P-3 Velour Matte and P-C Level HaircellImpact resistantEasy to form with good part definiti.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 64.4 °C | 148 °F | ASTM D648 |
Asahi Kasei Thermylene® P6-20FG-0753 20% Glass Fiber Reinforced, Heat Stabilized Information provided by Asahi Thermofil |