Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 42.0 - 47.0 °C
108 - 117 °F
Average value: 44.3 °C Grade Count:51
Overview of materials for High Density Polyethylene (HDPE), Ultra High Molecular Weight
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Ultra High Molecular Weight". Each property range of values reported i..
Deflection Temperature at 1.8 MPa (264 psi) 46.0 - 47.0 °C
115 - 117 °F
ASTM D648-98c
DSM Somos® ProtoGen™ O-XT 18420 Epoxy Resin for Stereolithography, UV Postcure at HOC -2
DescriptionDSM Somos® ProtoGen O-XT 18420 is a liquid, ABS-like, photopolymer that produces accurate parts ideal for general purpose applications. ProtoGen resins are the first SL resins to demons..