Polymer Property : Deflection Temperature at 1.8 MPa (264 psi) = 112 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 44.4 °C
112 °F
ASTM D648
RheTech Products E204-01 High Density Polyethylene, Black
Applications: Electrical housingsUnderhood componentsConsumer GoodsInjection molding conditions reported in table.Information provided by RheTech Products.
Deflection Temperature at 1.8 MPa (264 psi) 44.4 - 96.1 °C
112 - 205 °F
Average value: 67.3 °C Grade Count:46
Overview of materials for Polypropylene with 40% Calcium Carbonate (CaCO3) Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Calcium Carbonate (CaCO3) Filler". Specific grades with primary filler content be..
Deflection Temperature at 1.8 MPa (264 psi) 44.4 °C
112 °F
ASTM D648B
ExxonMobil HDPE HD 6704.18 High Density Polyethylene Copolymer Resin
Product Description: HD 6704 is a narrow molecular weight hexane copolymer designed for outstanding balance of ESCR, Toughness and Stiffness properties. This resin is ideally suited for heavy-duty a..
Deflection Temperature at 1.8 MPa (264 psi) 44.4 °C
112 °F
ASTM D648
RheTech Products E204-00 High Density Polyethylene, Natural
Applications: Electrical housingsUnderhood componentsConsumer GoodsInjection molding conditions reported in table.Information provided by RheTech Products.
Deflection Temperature at 1.8 MPa (264 psi) 44.4 °C
112 °F
ASTM D648
Spartech PP7240 Calcium Carbonate Filled High Impact Copolymer
Provides the highest level of impact of all copolymers and are useful in applications where improved processing and stiffness are required versus unfilled copolymer materials.Information provided by..