Polymer Property : Beta Transus = 1913 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Beta Transus 1045 °C
1913 °F
TIMET TIMETAL® 834 (Ti-5.8Al-4Sn-3.5Zr-0.7Nb-0.5Mo-0.35Si-0.06C) Titanium Alloy
High-Strength, High Temperature, Creep Resistant AlloyIndustry Specifications: France: T-A6EZ r4Nb.Features: TIMETAL 834 is a near alpha titanium alloy offering increased tensile strength and creep..