Thermal Properties | Metric | English | Comments |
---|---|---|---|
Beta Transus | 945 °C | 1730 °F | |
TIMET 6-6-2 Titanium Alloy (Ti-6Al-6V-2Sn), Solution Treated and Aged Features: TIMETAL 6-6-2 offers improved strength properties and greater depth hardenability compared with TIMETAL 6-4.Data provided by TIMET. |