Thermal Properties Metric English Comments
Deflection Temperature at 8.0 MPa 103 - 157 °C
217 - 315 °F
Average value: 134 °C Grade Count:4
Overview of materials for Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled". Specific grades with glass content between 15% an..