Polymer Property : Deflection Temperature at 8.0 MPa = 162 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 8.0 MPa 72.0 °C
162 °F
ISO 75-1/-2
Lanxess Pocan® TS 3220 901510 PBT + PET, 20% Glass Fiber
PBT+PET, 20% glass fibers, injection molding, impact modified, low tendency to warp, improved surface finish