Polymer Property : Flame Spread = 10.0 mm/min Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Flame Spread 10.0 mm/min

@Thickness 2.00 mm
0.394 in/min

@Thickness 0.0787 in
FMVSS Buring Speed
Eurostar Staramide AG3K PA66, 15% Glass Filled, Injection Molded
AG3K is a Heat and Hydrolytically Stabilized, 15% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppl..
Flame Spread 10.0 mm/min

@Thickness 2.00 mm
0.394 in/min

@Thickness 0.0787 in
FMVSS Buring Speed
Eurostar Staramide AG4 PA66, 20% Glass Filled, Injection Molded
AG4 is a 20% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
Flame Spread 10.0 mm/min

@Thickness 2.00 mm
0.394 in/min

@Thickness 0.0787 in
FMVSS Buring Speed
Eurostar Staramide AG4K PA66, 20% Glass Filled, Injection Molded
AG4K is a Heat and Hydrolytically Stabilized, 20% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppl..
Flame Spread 10.0 mm/min

@Thickness 2.00 mm
0.394 in/min

@Thickness 0.0787 in
FMVSS Burning Speed
Eurostar Staramide BG7H PA6, 35% Glass Fiber Filled, Heat Stabilized, Injection Molded
Staramide BG7H is a Heat Stabilized, 35% Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar.
Flame Spread 10.0 mm/min

@Thickness 2.00 mm
0.394 in/min

@Thickness 0.0787 in
FMVSS Burning Speed
Eurostar Staramide BG7HU PA6, 35% Glass Fiber Filled, Heat and UV Stabilized, Injection Molded
Staramide BG7H is a Heat and UV Stabilized, 35% Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar.
Flame Spread 10.0 mm/min

@Thickness 2.00 mm
0.394 in/min

@Thickness 0.0787 in
FMVSS Buring Speed
Eurostar Staramide AG3 PA66, 15% Glass Filled, Injection Molded
AG3 is a 15% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
Flame Spread 10.0 mm/min

@Thickness 2.00 mm
0.394 in/min

@Thickness 0.0787 in
FMVSS Burning Speed
Eurostar Staramide PF007 PA6, 35% Glass Fiber Filled, Injection Molded
Staramide PF007 is a 35% Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar.