Thermal Properties Metric English Comments
Brittleness Temperature -118 - 76.0 °C
-180 - 169 °F
Average value: -79.3 °C Grade Count:48
Overview of materials for High Density Polyethylene (HDPE), Extruded
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Extruded". Each property range of values reported is minimum and maxim..