Polymer Property : Brittleness Temperature = 46.4 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Brittleness Temperature 8.00 °C
46.4 °F
Colorite Polymers 9811 Clear Extrusion Vinyl Compound
Description: Clear non-toxic vinyl compounds are utilized by the health and medical industries for the extrusion of various components for the production of devices. The vinyl components used in pre..
Brittleness Temperature 8.00 °C
46.4 °F
Colorite Polymers 9812 Clear Injection Molding Vinyl Compound
Description: Clear non-toxic vinyl compounds are utilized by the health and medical industries for injection molding of various components such as drip chambers, connectors, valves, etc. The vinyl c..