Thermal Properties Metric English Comments
Brittleness Temperature -60.0 - 35.0 °C
-76.0 - 95.0 °F
Average value: -30.4 °C Grade Count:146
Overview of materials for PVC, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Extruded". Each property range of values reported is minimum and maximum values of appropriate MatW..