Polymer Property : Brittleness Temperature = 3.02 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Brittleness Temperature -16.1 °C
3.02 °F
ASTM D746
PolyOne Geon™ Vinyl Flexible C5D01 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Brittleness Temperature -16.1 °C
3.02 °F
ASTM D746
PolyOne Geon™ Vinyl Flexible G92B Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne