Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | -3.89 °C | 25.0 °F | ASTM D746 |
PolyOne Geon™ HC 2195G Polyvinyl Chloride, Flexible (PVC, Flexible) Geon HC 2195G is a 95 Shore A non-phthalate, gamma-stable flexible vinyl compound made from FDA sanctioned ingredients. HC 2195G can be used for extrusion and injection molding healthcare applicatio.. |
|||
Brittleness Temperature | -3.89 °C | 25.0 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible R148CE Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |