Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | <= 50.0 °C | <= 122 °F | ASTM D746 |
S&E Specialty Polymers TufGuard E™ XP-115DD-Zeta PE, Flame Retardant Application: Chlorinated PE TPO based compound suitable for Wire and Cable applications.Information provided by S&E Specialty Polymers |
|||
Brittleness Temperature | <= 50.0 °C | <= 122 °F | ASTM D746 |
S&E Specialty Polymers TufGuard E™ XP-115D-Zeta PE, Flame Retardant Application: Chlorinated PE TPO based compound suitable for Wire and Cable applications.Information provided by S&E Specialty Polymers |