Thermal Properties Metric English Comments
Brittleness Temperature -34.0 - -17.0 °C
-29.2 - 1.40 °F
Average value: -22.7 °C Grade Count:7
Overview of materials for Polybutene
This property data is a summary of similar materials in the MatWeb database for the category "Polybutene". Each property range of values reported is minimum and maximum values of appropriate MatWeb ..