Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Brittleness Temperature 0.500 °C
32.9 °F
molding, notched; ASTM D746
LyondellBasell Petrothene® NA967000 Low Density Polyethylene, Film Extrusion Grade
Petrothene NA967000 is a low density polyethylene resin designed for blown film, general purpose and industrial packaging applications. NA967000 exhibits good processing characteristics and impact s..