Thermal Properties Metric English Comments
Brittleness Temperature -85.0 - 0.000 °C
-121 - 32.0 °F
Average value: -52.5 °C Grade Count:80
Overview of materials for Low Density Polyethylene (LDPE), Molded
This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Molded". Each property range of values reported is minimum and maximum ..