Polymer Property : Brittleness Temperature = 0.000 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Brittleness Temperature <= 0.000 °C
<= 32.0 °F
ASTM D746
Polimeri Europa Riblene® MV 10 Low Density Polyethylene - Injection Molding
Riblene MV 10 is a low density polyethylene resin (LDPE) having an excellent fluidity.Parts made with Riblene MV 10 are highly flexible.Main Applications: Riblene MV 10 is ideal for injection moldi..
Brittleness Temperature <= 0.000 °C
<= 32.0 °F
ASTM D746
Polimeri Europa Riblene® MV 10 R Low Density Polyethylene - Injection Molding
Riblene MV 10 R is a low density polyethylene resin (LDPE) having an excellent fluidity.Parts made with Riblene MV 10 R are highly flexible.Main Applications: Riblene MV 10 R is ideal for injection..
Brittleness Temperature <= 0.000 °C
<= 32.0 °F
ASTM D746
Polimeri Europa Riblene® MY 00 Low Density Polyethylene - Injection Molding
Riblene MY 00 is a very high flowability low density polyethylene resin (LDPE).Main Applications: Riblene MY 00 is suitable for hot melts.Information provided by Polimeri Europa.
Brittleness Temperature 0.000 °C
32.0 °F
ASTM D746
PolyOne Geon™ Vinyl Flexible 1351 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Brittleness Temperature 0.000 °C
32.0 °F
ASTM D746
PolyOne Geon™ Vinyl Flexible R148AE Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Brittleness Temperature 0.000 °C
32.0 °F
ASTM D746
PolyOne Geon™ Vinyl Flexible R1700L Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Brittleness Temperature 0.000 °C
32.0 °F
ASTM D746
PolyOne Geon™ Vinyl Flexible F78E Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Brittleness Temperature 0.000 °C
32.0 °F
ASTM D746
PolyOne Geon™ Vinyl Flexible R3578A Polyvinyl Chloride, Flexible (PVC, Flexible)
A semirigid Vinyl Compound designed for edgeband applications with low migration characteristics.Information provided by PolyOne
Brittleness Temperature >= 0.000 °C
>= 32.0 °F
ASTM D746A
Solvay Specialty Polymers Solef® 3108/0903 Anti-static PVDF Compound  (discontinued **)
Key features of this grade: Anti-static, Formulated. Recommended processing is injection. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinated semi-crystall..
Brittleness Temperature >= 0.000 °C
>= 32.0 °F
ASTM D746A
Solvay Specialty Polymers Solef® 3208/0150 Anti-friction PVDF Compound  (discontinued **)
Key features of this grade: Anti-friction, Formulated. Recommended processing is injection. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinated semi-crysta..
Brittleness Temperature >= 0.000 °C
>= 32.0 °F
ASTM D746A
Solvay Specialty Polymers Solef® 8808/0902 Carbon Fiber Reinforced PVDF Compound  (discontinued **)
Key features of this grade: Carbon Fiber Reinforcement, Formulated. Recommended processing is injection. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinate..
Brittleness Temperature 0.000 - 10.0 °C
32.0 - 50.0 °F
ASTM D746A
Solvay Specialty Polymers Solef® 1008 PVDF Homopolymer  (discontinued **)
Key features of this grade: Low Viscosity, All Purpose, Injection, Virgin. Recommended processing is injection. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF ..
Brittleness Temperature 0.000 - 10.0 °C
32.0 - 50.0 °F
ASTM D746A
Solvay Specialty Polymers Solef® 1009 PVDF Homopolymer  (discontinued **)
Key features of this grade: Mean Viscosity, All Purpose, Injection/Extrusion, Virgin. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SO..
Brittleness Temperature 0.000 - 10.0 °C
32.0 - 50.0 °F
ASTM D746A
Solvay Specialty Polymers Solef® 1010 PVDF Homopolymer  (discontinued **)
Key features of this grade: Med Viscosity, All Purpose, Extrusion, Virgin. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF ..
Brittleness Temperature 0.000 - 10.0 °C
32.0 - 50.0 °F
ASTM D746A
Solvay Specialty Polymers Solef® 1012 PVDF Homopolymer  (discontinued **)
Key features of this grade: High Viscosity, Virgin. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinated semi-c..
Brittleness Temperature 0.000 °C
32.0 °F
ASTM D746
PolyOne Geon™ Vinyl Flexible R349AE Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne