Polymer Property : Brittleness Temperature = -95.0 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Brittleness Temperature <= -70.6 °C
<= -95.0 °F
ASTM D746
Network Polymers NPP 50-0158
Description: High Density Polyethylene (HDPE)Information provided by Network Polymers Inc.
Brittleness Temperature <= -70.6 °C
<= -95.0 °F
ASTM D746
Network Polymers NPP 50-1052
Description: High Density Polyethylene (HDPE)Information provided by Network Polymers Inc.
Brittleness Temperature <= -70.6 °C
<= -95.0 °F
ASTM D1525
Network Polymers NPP 50-2053
Description: High Density Polyethylene (HDPE)Information provided by Network Polymers Inc.
Brittleness Temperature <= -70.6 °C
<= -95.0 °F
ASTM D746
ExxonMobil HD 6761.17 Injection Molding Resin  (discontinued **)
HD 6761 is a narrow molecular weight hexene copolymer designed for good processability and excellent balance of ESCR, Toughness, and Stiffness properties. This resin is ideally suited for a heavy-d..