Polymer Property : Brittleness Temperature = -86.0 °C
Polymer Property :
Brittleness Temperature =
-86.0 °C
Product List
Thermal Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties
Metric
English
Comments
Brittleness Temperature
<=
-86.0
°C
<=
-123
°F
ASTM D746
Teknor Apex ELEXAR® EL 8421 Thermoplastic Elastomer
Information provided by Teknor Apex Company