Polymer Property : Brittleness Temperature = -72.2 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Brittleness Temperature -72.2 °C
-98.0 °F
ASTM D746
LyondellBasell Microthene® MP574189 Linear Low Density Polyethylene, Injection Molding Grade
ApplicationsMicrothene MP574189 exhibits excellent flow and impact with good stiffness. Typical applications include lids, closures, containers, housewares and medical items. MP574189 is 16 mesh pow..
Brittleness Temperature -72.2 °C
-98.0 °F
Molded and tested in accordance with ASTM D4976; ASTM D746
Dow DMDA-8940 NT 7 High Density Polyethylene Resin
DOW DMDA-8940 NT 7 is produced using UNIPOL™ process technology. It is intended for use in a broad range of injection molding applications such as housewares, toys, food containers and pails. Info..