Thermal Properties Metric English Comments
Brittleness Temperature -66.7 °C
-88.0 °F
ASTM D 746
CPT C-Flex® R70-082 Clear Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..