Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | -62.2 °C | -80.0 °F | ASTM 746 |
ExxonMobil Vyram™ 9101-75 Thermoplastic Elastomer
(discontinued **) A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing characteristi.. |
|||
Brittleness Temperature | -62.2 °C | -80.0 °F | ASTM D 746 |
CPT C-Flex® R70-081 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Brittleness Temperature | -62.2 °C | -80.0 °F | ASTM D746 |
ExxonMobil Santoprene® 211-45 Thermoplastic Elastomer A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
Brittleness Temperature | -62.2 °C | -80.0 °F | ASTM D746 |
ExxonMobil Santoprene® 8211-45 Thermoplastic Elastomer A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in dif.. |
|||
Brittleness Temperature | -62.2 °C | -80.0 °F | ASTM D746 |
ExxonMobil Santoprene® 8211-55 Thermoplastic Elastomer A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in dif.. |
|||
Brittleness Temperature | -62.2 °C | -80.0 °F | ASTM D746 |
ExxonMobil Santoprene® 8221-70 Thermoplastic Elastomer A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide.. |
|||
Brittleness Temperature | <= -62.2 °C | <= -80.0 °F | ASTM D 746 |
CPT C-Flex® R70-085 Clear Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Brittleness Temperature | -62.2 °C | -80.0 °F | ASTM D746; ISO 812 |
Advanced Polymer Alloys Alcryn® 4670 BK Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |
|||
Brittleness Temperature | -62.2 °C | -80.0 °F | ASTM 746 |
ExxonMobil Vyram™ 9201-75 Thermoplastic Elastomer
(discontinued **) A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing character.. |
|||
Brittleness Temperature | -62.2 °C | -80.0 °F | ASTM D746 |
ExxonMobil Santoprene® 111-45 Thermoplastic Elastomer A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |