Polymer Property : Brittleness Temperature = -6.00 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Brittleness Temperature -60.0 - -6.00 °C
-76.0 - 21.2 °F
Average value: -24.6 °C Grade Count:100
Overview of materials for Thermoset Fluoroelastomer
This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Fluoroelastomer". Each property range of values reported is minimum and maximum values of appr..