Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | -48.3 °C | -54.9 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible XV3816 Polyvinyl Chloride, Flexible (PVC, Flexible) NOTE: All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of.. |