Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | -31.7 °C | -25.1 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible B8000 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Brittleness Temperature | -31.7 °C | -25.1 °F | ASTM D746 |
PolyOne Geon™ HC 2170 Polyvinyl Chloride, Flexible (PVC, Flexible) Geon HC 2170 is a 70 Shore A non-phthalate flexible vinyl compound made from FDA sanctioned ingredients. HC 2170 can be used for extrusion and injection molding healthcare applications.NOTE: All ing.. |
|||
Brittleness Temperature | -31.7 °C | -25.1 °F | ASTM D746 |
PolyOne Geon™ HC 2170G Polyvinyl Chloride, Flexible (PVC, Flexible) Geon HC 2170G is a 70 Shore A non-phthalate, gamma-stable flexible vinyl compound made from FDA sanctioned ingredients. HC 2170G can be used for extrusion and injection molding healthcare applicatio.. |
|||
Brittleness Temperature | -31.7 °C | -25.0 °F | ASTM D746 |
Teknor Apex APEX® 80880-A Polyvinyl Chloride Compound Notes: UL Component Recognized Insulation Compound Uses: AWM Insulation Temperature Rating: 105°C Oil Rating: 60°CInformation Provided by Teknor Apex |