Thermal Properties Metric English Comments
Brittleness Temperature -28.1 °C
-18.6 °F
ASTM D746
PolyOne Geon™ Vinyl Wire & Cable Y594B Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne