Thermal Properties Metric English Comments
Brittleness Temperature -21.1 °C
-5.98 °F
ASTM D746
PolyOne Geon™ Vinyl Flexible A5D00 Polyvinyl Chloride, Flexible (PVC, Flexible)
Recommended for interior applications.Information provided by PolyOne
Brittleness Temperature -21.1 °C
-5.98 °F
ASTM D746
PolyOne Geon™ Vinyl Flexible A5DU0 Polyvinyl Chloride, Flexible (PVC, Flexible)
Recommended for interior applications.Information provided by PolyOne
Brittleness Temperature -21.1 °C
-5.98 °F
ASTM D746
PolyOne Geon™ Vinyl Flexible A5DUB Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Brittleness Temperature -21.1 °C
-5.98 °F
ASTM D746
PolyOne Geon™ Vinyl Flexible R264AE Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Brittleness Temperature -21.1 °C
-5.98 °F
ASTM D746
PolyOne Geon™ Vinyl Flexible R354AE Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Brittleness Temperature -21.1 °C
-6.00 °F
ASTM D746-95
Saint-Gobain Tygon® R-3400 UV Resistant Tubing Formulation
Tygon® R-3400: Ideal for virtually any permanent or temporary chemical transfer application, Tygon® UV Resistant Tubing combines suppleness and flexibility with resistance to a wide range of..
Copyright © lookpolymers.com All Rights Reserved