Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | <= -180 °C | <= -292 °F | ASTM D746 |
Chevron Phillips Marlex® C590 High Density Polyethylene
(discontinued **) High Density PolyethyleneData provided by Chevron Phillips Chemical Company, LP. |