Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | -79.0 °C | -110 °F | ASTM D746 |
Chevron Phillips Marlex® C579 High density polyethylene
(discontinued **) Benefits: outstanding impact and creep resistance, excellent ESCR, excellent chemical resistanceApplications: multi-layer fuel tanks, mono-layer fuel tanks, industrial bulk containersInformation pro.. |
|||
Brittleness Temperature | -79.0 °C | -110 °F | ASTM D746 |
Ashley Polymers Ashlene® 528L Nylon 66 General purpose injection molding grade.Data provided by the manufacturer |
|||
Brittleness Temperature | -79.0 °C | -110 °F | ASTM D746 |
Ashley Polymers Ashlene® 528LW Nylon 66 General purpose injection molding grade.Data provided by the manufacturer |
|||
Brittleness Temperature | -78.9 °C | -110 °F | ASTM D746; ISO 812 |
Advanced Polymer Alloys Alcryn® 2070 BK Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |
|||
Brittleness Temperature | -79.0 °C | -110 °F | |
Ascend Performance Materials VYDYNE® 21SP Nylon, General Purpose 1.4% Deformation under 14 MPa (2000 psi) load.Typical property data. VYDYNE is a registered trademark of Solutia Inc. |