Polymer Property : Distillation Temperature = 56.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Distillation Temperature 44.0 - 56.0 °C
111 - 133 °F
0.95
Unipetrol C5 Fraction
C5 fraction is mixture of mainly alifatic and cyclic hydrocarbons C5. It is colourless, volatile, extremely combustible and easily inflammable liquid with characteristic odour. It generates as a by-..