Thermal Properties | Metric | English | Comments |
---|---|---|---|
Distillation Temperature | <= 185 °C | <= 365 °F | 0.9 |
Unipetrol C9 Fraction Redistillated C9 fraction redistillated (RC9) is a distillation cut of pyrolysis gasoline, produced as a by-product during manufacture of ethylene. It is a transparent, colourless to yellowish liquid with prevail.. |