Thermal Properties | Metric | English | Comments |
---|---|---|---|
Working Point | 1165 °C | 2129 °F | Viscosity 10<sup>4</sup> dPa s; ISO 7884-2 |
Schott DUROBAX® amber Neutral Glass Tubing Neutral glass tubing, chemically highly resistant, with light protection Containers, test tubes, pipettes, chemical and technical apparatus The heavy metal content for the elements lead, cadmium, .. |
|||
Working Point | 1165 °C | 2129 °F | Viscosity 10<sup>4</sup> dPa s |
Schott FIOLAX® amber Neutral Glass Tubing Neutral glass tubing, chemically highly resistant, with light protection Pharmaceutical primary packagingInformation provided by SCHOTT AG. |