Polymer Property : Working Point = 1985 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Working Point 1085 °C
1985 °F
Viscosity 10<sup>4</sup> dPa s; ISO 7884-2
Schott Glass 8337B Borosilicate Glass
Borosilicate glass for sealing to Kovar metal and tungsten, highly UV-transmitting photomultiplier and UV detectors The heavy metal content for the elements lead, cadmium, mercury, and hexavalent ..