Thermal Properties Metric English Comments
Working Point 1023 °C
1873 °F
Viscosity 10<sup>4</sup> dPa s; ISO 7884-2
Schott Glass 8625 Biocompatible Glass
Biocompatible glass, high IR-absorbing, Transponders (implantable) The heavy metal content of the elements lead, cadmium, mercury, and hexavalent chromium is below 100 ppmInformation provided by S..