Thermal Properties | Metric | English | Comments |
---|---|---|---|
Working Point | 885 °C | 1630 °F | Viscosity 10<sup>4</sup> dPa s; ISO 7884-2 |
Schott Glass 8650 Sealing Glass Sealing glass for molybdenum, free from Na and K, of high lead content Implosion diodesInformation provided by SCHOTT AG. |