Thermal Properties Metric English Comments
Working Point 760 °C
1400 °F
Viscosity 10<sup>4</sup> dPa s; ISO 7884-2
Schott Glass 8532 Soft Glass
Soft glass, free from Na, of high lead content, lower sealing temperature than glass 8531, high dielectric constant Encapsulation of semiconductor components at low temperature (diodes)Information ..
Working Point 760 °C
1400 °F
Schott S8808 Contrast Enhancement Filter
Contrast Enhancement FilterInformation Provided by SCHOTT North America, Inc.